Mixed Results For Tio2 Feedstock Production From Major Producers

Titanium dioxide (TiO2) feedstock producer Sierra Rutile saw production for ilmenite increase in Q2 2014, compared with 2013, as it continued to upgrade its facilities. The company produced over 27,000 tonnes rutile during the quarter, a 3% increase year-on-year.