Mixed Barium-Lead Borate Glasses Studied By Optical And Vibrational Spectroscopy

Glasses of the ternary lead-barium borate series (70-x) B2O3-30 BaO-xPbO with x=0.05 to 30 mol% were studied for their optical properties by photoluminescence (PL) and UV-Vis absorption spectroscopy.

Author
Un-named
Origin
Unknown
Journal Title
Applied Glass Science 10 3 July 2019 339-348