Minimising The Environmental Impact Of Vehicle End-Of-Life Glass Recycling

In the first part of this article, the technologies for obtaining recyclable plastic-free glass and polymers that are already available were illustrated. This second part, reports the results of long term trials in polymer separation from glass, in the use of "glassy sand" for glass container production and in polymer cracking for hydrocarbon C1-C6 production.

Author
P Ercole Et Al
Origin
Ativ, Italy
Journal Title
Glass Worldwide Nov-Dec 2007 56-58
Sector
Flat glass
Class
F 2432