Mineralogical Characterization Of Ceramic Raw Materials By Powder Quantiative X-Ray Diffraction Methods (In Spanish)

The aim of this work is to characterize mineral phases present in raw material employed in the ceramic industry. In this way, two quantitative X-ray diffraction methods have been used, the Rietveld and the standardless methods. The results obtained are compared with the corresponding chemical analyses and calculated normative composition.

Author
M M Reventos Et Al
Origin
Universitat De Valencia, Spain
Journal Title
Bol Soc Esp Ceram Vidrio 41 6 2002 509-512
Sector
Glass Ceramics
Class
GC 484

Request article (free for British Glass members)

Mineralogical Characterization Of Ceramic Raw Materials By Powder Quantiative X-Ray Diffraction Methods (In Spanish)
Bol Soc Esp Ceram Vidrio 41 6 2002 509-512
GC 484
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
8 + 12 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.