Mineral Wool Primary Layer Structure Influence On The Fibre Distribution In The Final Product

A novel method of measuring and controlling the primary layer quality in a mineral wool production process is presented. The measurement method is based on image acquisition and processing of the mineral wool primary layer structure. As a statistical estimator of the primary layer quality, a ratio of root mean square (RMS) and average intensity in a selected region of the image was used. A regression model of the mineral wool production process control is presented. The final product local density of mineral wool as a function of the primary layer statistical estimators is analysed. The key process parameters are also taken into consideration. The regression model was derived using dimensional analysis and a selection of characteristic numbers. Results give good agreement with a regression coefficient higher than 0.92.

Author
D Dimovski Et Al
Origin
Renault Sa, France
Journal Title
Glass Technology 45 4 2004 175-181
Sector
Glass Fibre
Class
GF 422

Request article (free for British Glass members)

Mineral Wool Primary Layer Structure Influence On The Fibre Distribution In The Final Product
Glass Technology 45 4 2004 175-181
GF 422
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
13 + 7 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.