The Migration Of Lead From Lead Crystal Glasses (German)

The migration of lead from various lead crystal glasses into wine is studied using a graphite - furnace - AAS. The increase in lead concentration with increasing exposure time is described using mathematical relationships.

Author
M Haldimann, B Zimmerli
Origin
Bundesamt Fur Gesundheitswesen, Bern
Journal Title
Mitt. Giebiete Lebensm. Hyg. 1991 82 278 -289