The Microstructure-Property Correlation Of Synthetic Granite Tiles Developed From Beach Sand Garnet

In this study, garnet sand which is a by-product of beach sand minerals, was utilised as a major raw material to develop single fired "synthetic granite" tiles. A series of compositions containing garnet sand, clay & feldspar were studied by heating at different temperatures. A hard vitrified product with dense microstructure/low porosity was obtained in the temp range of 1100-1150 deg C from an optimum combination. XRD study on the vitrified samples showed the presence of mullite, ferrite spinel & monticellite as major phases. Presence of these phases contributed towards superior hardness, abrasion resistance & strength development. SEM studies revealed the presence of strongly interlocked crystals of mullite & feroan spinel embedded in an amorphous glassy phase. Superior physico-mechanical properties may replace natural granite tiles in building industries.

Author
D K Das Et Al
Origin
Cgcri, India
Journal Title
Trans Ind Ceram Soc 62 1 2003 27-30
Sector
Glass Ceramics
Class
GC 549

Request article (free for British Glass members)

The Microstructure-Property Correlation Of Synthetic Granite Tiles Developed From Beach Sand Garnet
Trans Ind Ceram Soc 62 1 2003 27-30
GC 549
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 4 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.