Microstructure And Mechanical Properties Of Friction Stir Welded Joint Of Zr46Cu46A18 Bulk Metallic Glass With Pure Aluminium

A 2mm thick Zr46Cu46A18 bulk metallic glass (BMG) plate and 4.5mm thick pure aluminum plate were successfully joined by friction stir welding (FSW), and the defect-free BMG/A1 joint is produced. Some BMG particles were stirred into the aluminum side in the stir zone and reacted with the Al to form the Al-rich phase. The residues of the BMG particles still maintained the amorphous structure. However, no crystallization and reaction layer are detected at the interface between the BMG and Al. The ultimate tensile strength of the joint is about 190 MPa, which reaches up to 92% of the pure aluminum matrix.

Author
F P Li Et Al
Origin
Xiangtan University, Hunan, China
Journal Title
Mat Sci Eng A 588 2013 196-200
Sector
Special Glass
Class
S 4091

Request article (free for British Glass members)

Microstructure And Mechanical Properties Of Friction Stir Welded Joint Of Zr46Cu46A18 Bulk Metallic Glass With Pure Aluminium
Mat Sci Eng A 588 2013 196-200
S 4091
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
8 + 9 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.