Microscopic Optical Components Made With A Rubber Stamp

Researchers at Lucent Technologies' Bell Labs have developed a technique for stamping sub-micron features on glass and other materials using a rubber stamp. The process involves making reusable rubber stamps with extremely small features, at times only a few hundred nanometers across. The stamps are made by pouring liquid rubber onto a prototype device made of patterned silicon. The rubber solidifies and is peeled away from the silicon, creaging a perfect reproduction of the microscopic silicon relief pattern. The technique is intended to be a cheaper alternative to conventional lithography and has the flexibility to print on curved surfaces, such as the outside of an optical fibre.

Author
Un-named
Origin
Unknown
Journal Title
Glass Industry 80 6 May 1999 7
Sector
News Items
Class
N 642

Request article (free for British Glass members)

Microscopic Optical Components Made With A Rubber Stamp
Glass Industry 80 6 May 1999 7
N 642
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.