Micromechanics Of Failure Waves In Glass: I, Experiments

Plate & bar impact experiments were performed on glass to investigate the mechanisms responsible for recently observed failure waves. Observations are reported showing that the so-called failure wave is actually a propagating boundary of damaged material. It inititates at the specimen surface, without appreciable incubation time, & propagates to its interior. In-material gauge measurements show that the spall strength & shear resistance are drastically reduced behind the failure wave front. Shear resistance interferometrically measured in pressure-shear experiments is in agreement with the in-material gauge records. Normal stress measurements performed close to the impact surface show a progressive reduction in normal stress behind the failure wave.

Author
H D Espinosa Et Al
Origin
Purdue University, Usa
Journal Title
J Am Ceram Soc 80 8 1997 2061-2073
Sector
General
Class
G 1701

Request article (free for British Glass members)

Micromechanics Of Failure Waves In Glass: I, Experiments
J Am Ceram Soc 80 8 1997 2061-2073
G 1701
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.