Microfloat Technology - A New Challenge For The Production Of High Tech Borosilicate Flat Glasses

Since the days of Otto Schott, the development of borosilicate glass has been a continously proceeding process to achieve higher quality and efficiency in special glass production that offers new potentials in the special glass application field. Because of its inexhaustible possibilites of compositional variations, special borosilicate glasses can meet extraordianry properites. This paper looks at the partnership between Schott and Asahi and the development of microfloat technology.

Author
K Schnieder Et Al
Origin
Jenaer Glaswerke, Germany
Journal Title
Schott Research 1993-1995 251-265
Sector
Flat glass
Class
F 736

Request article (free for British Glass members)

Microfloat Technology - A New Challenge For The Production Of High Tech Borosilicate Flat Glasses
Schott Research 1993-1995 251-265
F 736
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
9 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.