Mgo-Cao-Al2O3-Sio2 Glassy And Glass Ceramic Systems: The Effect Of Substitution Of Coo Or Nio In Place Of Mgo Or Cao

Nickel and cobalt were separately incorporated in MgO-CaO-Al2O3-SiO2 glasses. Their effect on the crystallisation phenomenon of the amorphous materials into a glass ceramic was investigated by means of thermal analysis and x-ray power diffraction.

Author
L Barbieri Et Al
Origin
University Of Modena, Italy
Journal Title
Phys Chem Glasses 36 4 1995 176-182