Mg Glass On Form (Norwegian)

A profile of the Norwegian glass company MG Glass is presented. Recent investments of 30 million kroner include a new electric feeder featuring computer control.

Author
R Johansen
Origin
Unknown
Journal Title
Emballering 1987 18 9 3-5
Sector
Container glass
Class
C 27

Request article (free for British Glass members)

Mg Glass On Form (Norwegian)
Emballering 1987 18 9 3-5