Mexico'S Container Glass Sector Continues To Rise

Mexico is one of the largest and fastest-growing container glass sectors in the world, spurred by its vibrant beer and tequila industries. Recent acquisitions, takeovers and new plant set-ups have made the country's container glass industry one of the world's most interesting, as reported in this article.