[Mexico] Vitro Increases Furnace Capacity In Queretaro

Vitro SAB de CV has announced that with an investment of US$ 50M to carry out major maintenance works on one of its furnaces in the Vidriera Queretaro Plant, it was able to convert the furnace into the largest of its kind in Latin America and to increase its container production capacity by 9%. Capacity of the plant is over 500/tpd. In the last 3 years alone, the company has invested US$ 120M have been invested to make major repairs on three furnaces to increase capacity and lengthen its life. Total production capacity for all furnaces is around 700/tpd.

Author
Un-named
Origin
Unknown
Journal Title
Gmpa 5/2013 28
Sector
Container glass
Class
C 5013

Request article (free for British Glass members)

[Mexico] Vitro Increases Furnace Capacity In Queretaro
Gmpa 5/2013 28
C 5013
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
10 + 10 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.