Methods For Testing Lubricity And Scratch Resistance Of Coated Glass Containers

This report presents methods for testing lubricity and scratch resistance of coated glass containers. Two tests for evaluating lubricating coatings on glass are: (i) Lubricity; and, (ii) Scratch. The first is essentially a measure of static coefficient of friction between glass containers under no load except their own weight. The second is a measure of static coefficient of friction between glass containers under no load except their own weight. The second is a measure of the load needed to develop glass-to-glass contact between two glass containers in sliding contact.

Author
Gmic
Origin
Glass Container Manufacturers Inst, Usa
Journal Title
Gmic Technical Bulletin No 64, 1965
Sector
Primary Papers
Class
PP 1520

Request article (free for British Glass members)

Methods For Testing Lubricity And Scratch Resistance Of Coated Glass Containers
Gmic Technical Bulletin No 64, 1965
PP 1520
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
6 + 12 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.