Methods Of Batch Analysis. Part 2 The Analysis Of A Lead Crystal Glass Batch

A detailed working procedure is given for determining the amounts of sand, red lead, potassium carbonate, and saltcake in batches for making potassium oxide-lead oxide-silica glasses.