Methods For The Analysis Of Ream Knots In Glass

Methods are described whereby the complete analysis of ream knots occurring in silica-soda-lime-magnesia glasses can be accomplished by the use of rapid methods. The sample usually consists of about 20mg of powdered glass obtained by drilling with a tungsten carbide drill. Silica is determined spectrophotometrically, a spectrographic method being employed for the determination of Fe2O3. Al2O3, TiO2, ZrO2, CaO, and MgO. A flame photometer is used for the determination of Na2O and K2O. Additional information on other elements present in minor or trace amounts can be obtained from the spectrographic analysis.

Author
W Ward & E Fletcher
Origin
Unknown
Journal Title
Glass Technology 4 1 1963 13-17
Sector
Primary Papers
Class
PP 1350

Request article (free for British Glass members)

Methods For The Analysis Of Ream Knots In Glass
Glass Technology 4 1 1963 13-17
PP 1350
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 12 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.