A Method For Estimating Heat-Sheilding Properties Of Mineral Wool Insulation Based On Silicate Fibrous Materials

A method for the estimation of the heat-shielding properties of gas-filled mineral wool insulators is considered which takes into account the mechanism of interrelated heat and mass transfer processes and their intensities depending on the service conditions, design specifics, and technological parameters of the insulating material.