Mesoporous Bioactive Glass Nanolayer-Modified Zirconia Coatings On Ti-6Al-4V With Improved In Vitro Bioactivity

The bioactivity of coatings on alloy implants plays critical roles in the fast osteointegration and maintenance of a long-term life span of the implants. The aim of this study is to incorporate nanopores and bioactive components into the plasma-sprayed coatings by constructing nanopores and bioactive elements on the surface of coatings and further improve their in vitro bone-forming activity. In this study, mesoporous bioactive glasses (MBG) were used for modifying the surface of ZrO2 coatings on Ti-6Al-4V by spin-coating methods. The result shows that the MBG nanolayer has been successfully coated on the surface of ZrO2 coatings.

Author
Y Zhang Et Al
Origin
Shanghai University, China
Journal Title
Int J Appl Glass Sci 7 2 2016 216-228
Sector
Special Glass
Class
S 4254

Request article (free for British Glass members)

Mesoporous Bioactive Glass Nanolayer-Modified Zirconia Coatings On Ti-6Al-4V With Improved In Vitro Bioactivity
Int J Appl Glass Sci 7 2 2016 216-228
S 4254
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.