[Melting] A Superior Melt With Molybdenum

According to the author of this paper, molybdenum is an excellent choice electrode material for glass melting applications. The chemical and metallurgical characteristics, along with the mechanical and physical properties of molybdenum, produce a higher quality glass melting electrode. Although molybdenum has enjoyed widespread use in glass melting for years, the high temperature metallurgical processing required to produce molybdenum glass melting electrodes has remained relatively unknown and limited to a few companies.

Author
T Dziobek
Origin
H C Stark, Usa
Journal Title
Glass Worldwide Sept-Oct/2011 74-76
Sector
General
Class
G 3940

Request article (free for British Glass members)

[Melting] A Superior Melt With Molybdenum
Glass Worldwide Sept-Oct/2011 74-76
G 3940
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 11 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.