[Melting] Innovative Casting Material Extends Furnace Floor Life

In this article the authors describe a reliable hot repair solution that allows glassmakers to continue operating furnaces after the furnace floor suffers an emergency leak or when the furnace floor is suspected of having severe damage and a potential glass leak may be imminent.