Medical Applications Of Zirconium Oxide Hybrid Materials

In this review the authors consider the use of zirconium oxide hybrid materials in tissue-engineering scaffolds, microscale valves, microfluidic devices, drug-screening devices, drug delivery devices, bone prostheses and other medical devices. Along these lines, also presented is a novel approach for processing zirconium oxide hybrid materials via two-photon polymerization.

Author
P R Miller Et Al
Origin
Unknown
Journal Title
Am Ceram Soc Bull 90 7 24-29