Mechanistic Analysis Of Time-Dependent Failure Of Oxynitride Glass-Joined Silicon Nitride Below 1000 Degrees C

Creep, devitrification, stress-aided oxidation-controlled slow crack growth, and viscous cavitation-controlled failure are examined as possible controlling mechanisms for time-dependent failure at elevated temperatures.