Volatilization of fluorine and boron compounds from E-glass melts containing up to 1.55 wt% fluorine was investigated in a flowing air atmosphere in the temperature range 1250 to 1350 deg C employing the transpiration method. The mass loss and the amounts of fluorine and B2O3 emitted were determined discontinuously as a function of time. The kinetics of B2O3 emission from fluorine-containing as well as fluorine-free E-glass melts can be approximated by the model of a first order process of B2O3 with water vapour from the atmosphere at the melt surface.

Author
C Pentzel
Origin
Unknown
Journal Title
Glastech Ber Glass Sci Technol 67 8 1994 213-219
Sector
Special Glass
Class
S 826

Request article (free for British Glass members)

Mechanism Of Volatilization Of Fluorides From E-Glass Melts
Glastech Ber Glass Sci Technol 67 8 1994 213-219
S 826
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
17 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.