Mechanism Of The Interaction Between Quartz Glasses And The Lubricant-Cooling In Grinding.

The mechanism of the reaction between metacide, which is a coolant-lubricant component, and quartz glass in the course of grinding is investigated. It is shown that in the absence of grinding, the main type of reaction between metacide and glass is formation of hydrogen bonds. Under the effect of mechanical action both the polymer and the glass surface are modified, and as a consequence, other types of reactions occur between glass and metacide.

Author
I A Gagina Etal
Origin
Institute Phys Chem Russian Acadamy
Journal Title
Glass And Ceramics 57 1-2 2000 8-10
Sector
Special Glass
Class
S 3147

Request article (free for British Glass members)

Mechanism Of The Interaction Between Quartz Glasses And The Lubricant-Cooling In Grinding.
Glass And Ceramics 57 1-2 2000 8-10
S 3147
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.