Mechanism Of Defect Creation On Sheet Glass By Particle Impact And Its Influence On Stray Light

Stray light on the windshields of automotive vehicles, caused by the impact of small particles, imposes severe safety hazards during night driving. Due to reduced contrast by stray light, non-illuminated objects are perceived much later than through pristine windshields. The objective of this paper is, therefore, to show the dependence of stray light on impact velocity, impact angle, particle shape and the mechanical properties of the impacting particle and the target material. Single and multiple impacts of SiC(~1mg/particle) and quartz sand (~0.7mg/particle) on ordinary and strengthened float glass under angles of 30, 45, and 90 degrees and velocities between 50 and 200 km/h were investigated. Profilometer and various methods of stray light measurement, such as total integrated scattering, were used.

Author
K Heinrich Holtmann Et Al
Origin
Universitat Clausthal, Germany
Journal Title
Glastech Ber Glass Sci Technol 71 8 1998 247-255
Sector
Flat glass
Class
F 860

Request article (free for British Glass members)

Mechanism Of Defect Creation On Sheet Glass By Particle Impact And Its Influence On Stray Light
Glastech Ber Glass Sci Technol 71 8 1998 247-255
F 860
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 10 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.