Mechanical Properties Of Optically Transparent Glass-Ceramics Containing Lithium Mica Nanocrystals

Optically transparent glass-ceramics that contain lithium mica nanocrystals of

Author
V Khani & P Alizadeh
Origin
Tarbiat Modares University, Tehran, Iran
Journal Title
Phys Chem Glasses 54 2 2013 104-108
Sector
Glass Ceramics
Class
GC 830