Mechanical Properties Of Microstructurable Glasses

Microstructurable glasses of the system Li20-Al203-Si02 are objects of research at the Ilmenau Technical University. These glasses also contain alkali oxides and dopants. The dopants are important for microstructuring. Main directions of research are: special glass materials, structuring technolgies, joining processes and applications. The glasses can be structured with a photolithographic process using; UV exposure, thermal treatment and etching. Using this process, it is possible to make holes, structures with a defined depth, structures with various depths and three-dimensional structures without undercut. Different glass sheets can be joined with a thermal process. Depending on the thermal expanison coefficient glass/metal compounds may be realized by microelectroplating.

Author
A Harnisch & D Hulsenberg
Origin
Unknown
Journal Title
Glastech Ber Glass Sci Technol 73 3 2000 67-72
Sector
Special Glass
Class
S 1898

Request article (free for British Glass members)

Mechanical Properties Of Microstructurable Glasses
Glastech Ber Glass Sci Technol 73 3 2000 67-72
S 1898
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.