The Mechanical Properties And Fracture Behaviour Of Some Chemically Strengthened Silicate And Borate Glasses

The treatment of a number of alkali magnesium aluminosilicate glasses ion exchanged in sodium or potassium nitrates are reported and the results discussed.

Author
I W Donald Et Al
Origin
Atomic Weapons Establishment, Uk
Journal Title
Glass Technology 34 3 1993 114-119
Sector
General
Class
G 914