Mechanical Model To Simulate Buildup And Relaxation Of Stress During Glass Chemical Strengthening

A mechanical model comprising Hookean springs and Newtonian dashpots in a series configuration of a Maxwell element and a Voigt–Kelvin element is used to simulate the buildup and relaxation of stresses during ion exchange of glass. The spectrum of time constants for the dashpots spans from picoseconds to years. Good consistency is developed with molecular dynamic simulations published earlier.

Author
A K Varshneya
Origin
Unknown
Journal Title
J Non Cryst Solids 433 1 Feb 2016 28-30
Sector
Special Glass
Class
S 4363

Request article (free for British Glass members)

Mechanical Model To Simulate Buildup And Relaxation Of Stress During Glass Chemical Strengthening
J Non Cryst Solids 433 1 Feb 2016 28-30
S 4363
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 5 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.