Mechanical Characterization Of Sol-Gel-Derived Silicon Oxycarbide Glasses

Silicon oxycarbide glasses have been fabricated, inthe shape of thin rods suitable for flexural test experiments, by phyrolysis in an inert atmosphere at 1000 deg C and 1200 deg C of sol-gel precursors containing Si-CH3 and Si-H bonds.

Author
G D Soraru Et Al
Origin
Universita De Trento, Italy
Journal Title
J Am Ceram Soc 79 8 1996 2074-2080
Sector
Special Glass
Class
S 1082

Request article (free for British Glass members)

Mechanical Characterization Of Sol-Gel-Derived Silicon Oxycarbide Glasses
J Am Ceram Soc 79 8 1996 2074-2080
S 1082