Mechanical Behaviour Of Glass Reinforced With Si02 Hybrid Sol-Gel Coatings

This paper reports on the preparation of coatings from different sols on amber beer bottles & soda-lime glass rods & slides by a dipping process. Various withdrawal rates & heat treatments (from 150-500 deg C) were used to prepare the coats in order to determine the best conditions as a function of composition. In all cases, transparent & crack-free coatings with good adhesion were obtained. Rods & slides of soda-lime glass were mechanically tested using four-point flexure & ring-on-ring tests. The results indicate that the TEOS/y-MPS coated rods & slides treated at 150 deg C show the best behaviour. In the case of beer bottles, two different types of container were used: untreated & protected bottles with a hot-end SnO2 coating. The bottles were tested using the normal standards of hollow glass: scratch resistance, sliding angle & internal pressure.

Author
S Pellice Et Al
Origin
Intema, Argentina
Journal Title
J Non-Cryst Solids 348 2004 172-179
Sector
Container glass
Class
C 2846b

Request article (free for British Glass members)

Mechanical Behaviour Of Glass Reinforced With Si02 Hybrid Sol-Gel Coatings
J Non-Cryst Solids 348 2004 172-179
C 2846b
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 7 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.