Measurement And Control Of Colour In Coloured Glass

This paper describes a method of measurement and control of coloured glass. The examples of measurement of colour, dominant wavelength, colour purity and colour brightness as well as control of colour for the coloured flatted glass are given by means of CIE1964, and also the control range of colour in the glass is presented.

Author
J Peilin & M Xiangde
Origin
Henan Zhenghua Glass Processing Factory, China
Journal Title
Proc Of Xvi Icg Beijing, China Vol7 1995 125-128
Sector
Special Glass
Class
S 1483

Request article (free for British Glass members)