Mathematical Modelling Of Glass Melting Furnace Design With Regard To Nox Formation

A three-dimensional mathematical model for turbulent flow and combustion on the basis of turbulence/chemistry interactions and radiative heat transfer taking into account spectral effects of surrounding walls and combustion gases is described.