Mathematical Modelling Of Glass Mass Flow In A Conventional Glass Tank Furnace Using Isotope Data

Mathematical models of a conventional glass tank furnace have been developed on the basis of isotope measurements. Partial or ordinary differential equations were used to describe the model.