Materials Recovery From Waste Cathode Ray Tubes (Crts)

The final report is presented for a project, undertaken by the Industry Council for Electronic Equipment Recycling (ICER), which aimed to examine potential applications for waste cathode ray tube (CRT) glass. The project also aimed to prepare for the implementation of the Waste Electrical and Electronic Equipment (WEEE) Directive in 2004. The report is downloadable from WRAP's website: www.wrap.org.uk