Marblite Facing Plates Based On Industrial Wastes

The possibility of making glass for facing materials from cullet and blast furnace slag, with no conventional batch materials included in the composition, has been demonstrated in trials on a 0.5 tonne/day day tank fired on natural gas. The Avtosteklo factory has produced samples for evaluation in the construction industry.