Manufacture Of Flat (Float) Glass

This invention relates to the manufacture of flat glass in ribbon.

Author
L.A.B. Pilkington And K. Bickerstaff, Pilkington Bros Ltd
Origin
Unknown
Journal Title
U.S.P. 2,911,759 10.11.59