Management Of Hot Waste Glass Recycling

With production rates and capacities of furnaces constantly increasing, equipment for hot glass recycling must be designed and dimensioned to facilitate maximum efficiency and minimum human intervention. To this end, Portuguese supplier Vidromecanica describes the benefits of its scraper conveyors for the effective management of hot waste glass recycling.