Luminescent Solar Concentrators: Effects Of Shape On Efficiency

The effects of shape and photovoltaic cell placement on efficiency are studied for luminescent solar concentrators. The mean path length of light rays is found to be a poor measure of performance. Simple arguments based on a method of images show that the efficiency grows linearly with detector size h, saturating at h-pA/?, where A is the captation area of the collector, and ? is the attenuation length of radiation in the medium. Monte Carlo simulations confirm that efficiency is relatively independent of collector geometry.

Author
E Loh & D J Scalapino
Origin
Unknown
Journal Title
Applied Optics 25 12 1986 1901-1907 Dx.Doi.org/10.1364/Ao.25.001901
Sector
Special Glass
Class
S 3816

Request article (free for British Glass members)

Luminescent Solar Concentrators: Effects Of Shape On Efficiency
Applied Optics 25 12 1986 1901-1907 Dx.Doi.org/10.1364/Ao.25.001901
S 3816
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 4 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.