Lubrication Practices In Glass Plants - 1991

Current progress in the application of lubrication and coating materials in glassworks is reviewed. Use of the most suitable materials for each area of glass production and the different ways of applying the lubricant are discussed.

Author
J T Golden
Origin
Renite Company
Journal Title
Glass Machinery Plants & Accessories 1991 4 2 76-81
Sector
General
Class
G 631