Lubrication - Mould Swabbing And Article Quality

Modern glass plants make huge demands on lubricants. Different formulations are needed for different glassmaking tasks, as explained here.

Author
C Pirazzi
Origin
Acheson, France
Journal Title
Glass March/05 62
Sector
Container glass
Class
C 2629

Request article (free for British Glass members)

Lubrication - Mould Swabbing And Article Quality
Glass March/05 62