Lower Sulphur Fuels

The market for fuel oil and the implications of the EC Directive which commits the UK to reduce emissions from existing plant above 50MW are discussed.

Author
C Swadkin
Origin
Shell (Uk) Ltd
Journal Title
Glass Technology 1991 32 3 68-70
Sector
General
Class
G 617

Request article (free for British Glass members)

Lower Sulphur Fuels
Glass Technology 1991 32 3 68-70
G 617