Low-Tg Phosphate Glasses With Improved Water Resistance For The Coating Of Fluoride Glass Fibres

Starting from a multicomponent lead phosphate glass composition given in the literature, a glass was developed suitable for the protective overclad of heavy-metal fluoride glass fibres. Besides a low glass transition temperature 18.10-6K-1, the phosphate glass material developed had a water resistance at 60 degC for 10h comparable to that of commercial container glass.

Author
M Hartmann Et Al
Origin
Inst Fur Nihchtmetallische Werkstoffe, Germany
Journal Title
Glastech Ber Glass Sci Technol 68 11 1995 352-359
Sector
Glass Fibre
Class
GF 142

Request article (free for British Glass members)

Low-Tg Phosphate Glasses With Improved Water Resistance For The Coating Of Fluoride Glass Fibres
Glastech Ber Glass Sci Technol 68 11 1995 352-359
GF 142
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.