Low-Temperature Thermal Properties Of Glass

It is a fundamental feature of amorphous materials like glasses that they exhibit a markedly different low-temperature behaviour than their crystalline counterparts in phonon-related properties. Below 1K the thermal, acoustic and dielectric properties show a characteristic temperature dependence (quasi-linear specific heat, quadratic thermal conductivity, logarithmic ultrasound velocity shift, logarithmic electric permittivity, etc) in all glasses independent of their chemical composition. These phonon-related low temperature anomalies can be explained phenomenologically by the tunneling model, which has provided a basic theoretical concept for the explanation of the characteristic features of glassy behaviours below 1K.

Author
P Strehlow
Origin
Physikalisch-Technische Bundesantalt, Berlin, Germany
Journal Title
Glastech Ber Glass Sci Technol 68 C1 1995 67-72
Sector
Special Glass
Class
S 1007

Request article (free for British Glass members)

Low-Temperature Thermal Properties Of Glass
Glastech Ber Glass Sci Technol 68 C1 1995 67-72
S 1007
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
10 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.