Low Temperature Additive Manufacturing Of Three Dimensional Scaffolds For Bone-Tissue Engineering Applications: Processing Related Challenges And Property Assessment

In the last two decades, additive manufacturing (AM) has made significant progress towards the fabrication of bio-materials and tissue engineering constructs. One direction of research is focused on the development of mechanically stable implants with patient-specific size/shape and another direction has been to fabricate tissue-engineered scaffolds with designed porous architecture to facilitate vascularization. Among AM techniques, 3D powder printing (3DPL) is based on extrusion of bio-polymers to create artificial tissues. This review aims to develop a better understanding of the science and engineering aspects of these low temperature AM techniques in the context of the bone-tissue engineering applications.

Author
A Kumar Et Al
Origin
Indian Inst Science, Bangalore, India
Journal Title
Materials Sci & Eng R103 2016 1-39
Sector
Special Glass
Class
S 4243

Request article (free for British Glass members)

Low Temperature Additive Manufacturing Of Three Dimensional Scaffolds For Bone-Tissue Engineering Applications: Processing Related Challenges And Property Assessment
Materials Sci & Eng R103 2016 1-39
S 4243
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
6 + 13 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.