Low Melting Pb0-Zn0-P205 Glasses

A series of lead zinc phosphate glasses containing 30-80 mol% P205, 0-60% PbO and 0-60% ZnO have been prepared and characterised.

Author
H S Liu Et Al
Origin
National Tsing Hua University, Taiwan
Journal Title
Phys Chem Glasses 37 6 1996 227-235
Sector
Special Glass
Class
S 1103