Low-Melting Mat Glazes For Artistic Ceramic Products

The results of synthesis of low-melting mat glazes in the R20-R0-B203-Al203-Ti02-Si02 system are presented. The relation between the physicochemical properties of the coatings and the phase composition and structure of the glazed glasses is investigated as a function of the heat treatment regime.

Author
I A Levitskii & S A Gailevich
Origin
Unknown
Journal Title
Glass & Ceramics 53 3-4 1996 78-81