Low-Fire Processing (Ca1-Xnd2X/3)Ti03 Microwave Ceramics

Effects of 3Zn0.2B203 (3Z2B) glass addition on densification and microwave properties of (Ca1-xNd2x/3)Ti03 (CNT-X) have been investigated.